Color coated plates are prone to cracking before welding. We should first understand the cause of the crack in order to identify the cause and avoid accidents.

The zinc layer near the groove of the color coated plate oxidizes (forms ZnO) and evaporates under the action of arc heat, emitting white smoke and steam, making it easy to generate pores in the weld seam. The higher the welding current, the more severe the zinc evaporation, and the greater the sensitivity of pores. When using titanium or titanium calcium welding rods for welding, it is not easy to produce pores within the medium current range. When using cellulose and low hydrogen welding rods for welding, it is easy to produce pores under low and high currents. In addition, the angle of the welding rod should be controlled within the range of 30° to 70°as much as possible.

Secondly, when using arc welding to weld color coated plates, the zinc layer near the molten pool oxidizes into ZnO and evaporates under the action of arc heat, forming a large amount of smoke and dust. Therefore, good ventilation measures should be taken. Under the same welding specifications, the amount of smoke generated by titanium oxide electrode welding is relatively low, while the amount of smoke generated by low hydrogen electrode welding is relatively large.

After the welding current of the color coated plate is low, the Zno formed during the heating process is not easy to overflow, which can easily cause Zno slag inclusion. Zno is relatively stable with a melting point of 1800 ℃. Large Zno slag inclusions have a very adverse effect on the plasticity of welds. When using titanium oxide welding rods, the distribution of Zno is fine and uniform, which has little effect on plasticity and tensile strength. When using cellulose or hydrogen welding rods, there is a large amount of Zno in the weld seam, resulting in poor weld performance

Author picture
Welcome To Share This Page:
Product Categories
Latest News
Get A Free Quote Now !
Contact Form Demo (#3)

Related Products

Related News

What are Galvanized Steel, Galvalume Steel, and Zinc Aluminum Magnesium Coated Steel? When you selecting coated steel for construction, roofing, and other applications, the choices

Over time, any type of metal is prone to rust or corrosion, which is inevitable. Protecting the surface of galvanized steel is crucial to extending

10 problems low price supplier Top 10 problems low price supplier when choosing a low-cost metal coil supplier may seem like an attractive way to

What is A36? A36 generally refers to ASTM A36, which is a widely used carbon steel material standard defined by the American Society for Testing

JIS G3322 JIS G3322 is Japanese Industrial Standard specifies the prepainted hot-dip 55% aluminium”zinc alloycoated steel sheet and strip .Hot dipped galvalume/aluzinc steel coil have better

What is Chromated Treatment? Chromated treatment involves immersing a metal object in a solution primarily composed of chromic acid or dichromate, resulting in the formation

What is Electro Galvanized Steel? What is galvanizing? Galvanizing refers to a rust-prevention method of attaching metallic zinc to the surface of iron or steel.

DX51D-Z120 Prepainted Galvanized Steel Coil   Introduction DX51D-Z120 prepainted galvanized steel coil is a building material widely used in various industries due to its enhanced

EN 10169 Table of Contents What is EN 10169? EN 10169 of this European Standard gives the specific requirements for continuously organic coated (coil coated)steel

Get A Free Quote Now!

If have any requests, please feel free to contact us, we will be eager to serve you.

Scroll to Top

GET A QUICK REQUESTS

Contact Form Demo (#3)
Open chat
Have a question ?
Powered WITOP Steel
Hi, Welcome, Get Free Quote Send us a message!
Only takes a few seconds to reach you.